To utilize oxidation-reduction reactions in the construction of a voltaic cell (chemical battery)
to study its properties.
Materials:
(2) 250-mL beakers
Paper towel
Electrodes
Voltmeter
1M aluminum nitrate
1M lead nitrate
1M sodium chloride
Procedure:
Attach the lead electrode to the negative side of the voltmeter and the copper electrode to the positive side.
Fill one beaker with Al(NO3)3 and the other with Pb(NO3)2.
Place the aluminum strip in the 1M Al(NO3)3 and the copper electrode in the 1M Pb(NO3)2 solution.
Prepare a salt bridge by soaking a rolled paper towel in the 1M NaCl solution. Put one end of the paper salt bridge in the 1M Al(NO3)3 solution and the other end in the 1M Pb(NO3)2 solution.
Allow the cell to run for a few minutes. Examine the two metallic electrodes during this period. The lead electrode should begin to dissolve and will become pitted. Aluminum metal will begin to form at the surface of the alumninum metal electrode.
After you have allowed the cell to run for a few minutes, disconnect the wires from the metallic electrodes.